Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

PQR-WPS overlay

Status
Not open for further replies.

1973Patrick

Petroleum
Aug 6, 2012
14

Dear all,

I have a GTAW semi-autom. WPS-PQR for overlay ER308L-ER309L on P1
Is it possible to create a new WPS for 309-316 on P1, based on the existing PQR without requalification?
Thnx! Patrick
 
Replies continue below

Recommended for you

You need to check the A number (QW-442) of 309-316 and compared to A number of 308L-309L. If they are the same, then you don't need requalification.
 
Re-qualification is unnecessary. The A-No for 316 is the same as 308.
 
Agreed. That however is not to say chemistry will meet your customer requirements. You may need to use a Mo bearing consumable for the first layer.
 