I am interested in finding a plating/coating for copper alloy 102. We have small copper parts. We need a very inexpesive plating that is corrosion resitant and is solderable. Does anyone have any suggestions?
 
Agreed, tin plating is the usual coating for copper when it needs to be soldered.
 