Am trying to use plastic shims between Aluminium Extruded bracket and concrete slab. I want to calculate the thickness and size of shims required for each bolt. Please support me
 
Replies continue below

Recommended for you

Make them thick enough so that pooled water doesn't bridge the gap. Make them large enough so that compressive stress doesn't cause creep. Use fiber reinforced plastics for better resistance to creep and cracking.
 
Welding, Bonding, Fastening ??

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 
I think the word "concrete" rules out welding or bonding as choices.
 