I am looking for standards or recommendations for maximum allowed torque for plastic screws, specifically for size 4-40 x ½ screw made of “peek” material ( Do these standards or recommendations exist?
I would appreciate if someone could share with this information.
 
Many times the maufacture of the screw will specify this in their documentation. This max. torque is also highly dependent on the size of the pilot hole.

Typically though #4-40 is a thread pitch for metal and #4-17 is for plastics,etc..

I would look into plastic thread forming screws like the hi-lo types or Plastite 45 from Reminc as they will allow a higher torque because thats what they are made for.

Here we torque a #4-17 screw into ABS using 7 in-lbs.
 
mcgyvr,

I think minchanin is asking for the torque required to drive a plastic machine screw into a previously tapped hole. The standard torque equation should answer this question. You can get the proof stress by reading up on the material.

T = KDF...

...where T is torque in inch pounds, D is major diameter in inches, and F is clamping force in pounds. The stress area of a 4-40UNC screw is 0.00604sq.in.

Does anyone know the friction factor K would be? I have all sorts of literature on metal bolts and screws, with and without lubrication. I have seen nothing on plastic.

JHG
 
Unreinforced (and without PTFE filler) PEEK against another part should have [μ] ~ 0.15.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Sorry I missed the "made of PEEK" and assumed going into PEEK..
 