Hi to everyone, I'm having a problem with an approved WPS for welding a 18" 7.92mm pipeline.
WPS have SMAW for the root and FCAW-S for the Fill and Cap. The first x-rays showed too many spatter in the bottom, that makes the film impossible to interpret. I know that this is a issue already known when using the SMAW process and not having access to the inside to clean. But now we are having a very big problem... can someone give me some advices?
WPS have SMAW for the root and FCAW-S for the Fill and Cap. The first x-rays showed too many spatter in the bottom, that makes the film impossible to interpret. I know that this is a issue already known when using the SMAW process and not having access to the inside to clean. But now we are having a very big problem... can someone give me some advices?