If you make the dissimilar weld using "B3" filler, lowering the PWHT temperature is recommended to mitigate carbon migration from the deposited weld metal to the P91 base material. Possibly the best method to make these welds is to use a "stabilized" (vanadium/niobium bearing) T23 or T24 type weld filler.