Manway necks are most commonly made from rolled plate. As JStephen says, the code allows, it is an economic decision. See API 650 4.5.2, which reads in part: "material for shell nozzles and shell manhole necks shall be seamless pipe, seamless forging, [highlight #FCE94F]or plate material[/highlight] as specified in 4.2.10.1."