Apr 16, 2024 #1 Hemal Chauhan Mechanical Joined Jan 24, 2024 Messages 4 Location IN Tank shell to neck joint welding permitted to Flush after PWHT? Regards, Hemal Chauhan 9909918636
Apr 16, 2024 #2 IFRs Petroleum Joined Nov 22, 2002 Messages 4,679 Location US In API 650 yes - see Figure 5.7.b. But, what does PWHT have to do with it? Upvote 0 Downvote
Apr 30, 2024 #3 Creed2023 Petroleum Joined Aug 14, 2023 Messages 6 Location AU to IFRs: I guess it relates to requirements of weld spacing, refer to Figure 5.6 Upvote 0 Downvote
May 6, 2024 #4 Dhurjati Sen Materials Joined Dec 14, 2017 Messages 1,001 Location IN Why the flushing was not carried out before PWHT? That is not a good fabrication practice, irrespective of what API permits. DHURJATI SEN Kolkata, India Upvote 0 Downvote
Why the flushing was not carried out before PWHT? That is not a good fabrication practice, irrespective of what API permits. DHURJATI SEN Kolkata, India