I recently completed a wood framed building that is going to be used as a retail building for a local farm. The building wasn't easy as the clients wanted large open spaces with vaulted ceilings and such (see my previous thread about scissor trusses from a few months ago). Everything was rushed during the design phase but we ended up getting the engineering completed and everyone was happy.
The other day I went out to the site to do a rough inspection of the completed framing. During my inspection I noticed a ton of that we had called out on the drawing missing. In all it seemed like the GC just used our drawings to pull a permit then decided to do whatever they wanted. Now we are in the fighting phase of the contract trying to get the items we called out on the drawings installed properly.... and running through the process of fixing their F**kups.
One particular items that is irking me has to do with the fact that we showed some 5 1/4" x 7" psl posts with an ABU base and a ECCQ cap that needed to be installed under some rather large truss girders. The GC decided to install 2 smaller posts to make the larger one (he installed the cap but not the base which is another issue). Barring other issues can you bolt together two smaller PSL posts to make a large post?
The other day I went out to the site to do a rough inspection of the completed framing. During my inspection I noticed a ton of that we had called out on the drawing missing. In all it seemed like the GC just used our drawings to pull a permit then decided to do whatever they wanted. Now we are in the fighting phase of the contract trying to get the items we called out on the drawings installed properly.... and running through the process of fixing their F**kups.
One particular items that is irking me has to do with the fact that we showed some 5 1/4" x 7" psl posts with an ABU base and a ECCQ cap that needed to be installed under some rather large truss girders. The GC decided to install 2 smaller posts to make the larger one (he installed the cap but not the base which is another issue). Barring other issues can you bolt together two smaller PSL posts to make a large post?