im a weder at jobcorps and need some information...i need to know where i can get information on welding symbols and blueprint reading. the information is for a final project.in order to go full time in welding...plz help.
 
hobart institute of welding technology in troy, ohio has a great self study program for symbols
 
Check AWS A 2.1 and AWS 2.4. these are the official standard welding symbols.
 
Hi Folks,
I just checked out the Royweb & Volvo links above. Whoa![bomb]. British and whatever are backwards!!. [shocked]I'm glad I got the education and I appreciate the sites for expanding my mind, but we should not have given that info to a welding student. It is incorrect for work in the USA.

AWS A2.4 is what is used here in the USA and you can often find the info in appendices to Lincoln or Miller handbooks for free.

A trick I use to keep things straight.

In the USA:

Above the reference line is "Other" side reference, not far side. Below the reference line is "Arrow" side. Arrow side information refers to the side of the joint to which the arrow points. Other side reference (above the line) refers to the side opposite the side of the joint to which the arrow points.

We are talking about the joint "interface". If I make a tee joint with the tee stem pointing up, the thickness of the stem makes my joint interface. The interface has two sides. Then I can make whatever weld configuration I want, like a complete-penetration bevel groove. A single bevel groove beveled from the other side has an arrow pointing to the joint with the welding symbol above the reference line. No prep where the arrow points.

Your welding instructor is probably better at the welding symbols than an engineer or detailer. Have fun!

Koz
 
The British drive on the wrong side of the road, and place weld marks on the wrong side of the arrow...
Makes sense to me.
 
I guess it looks good, too, if you are on the bottom side of the equator!