Feb 26, 2006 #1 HXLIU Mechanical Joined Dec 5, 2005 Messages 6 Location CN We have a OSBL sub-project of pumping seawater via CS pipeline. I want to know a safty and pratical method for lining and/or coating.
We have a OSBL sub-project of pumping seawater via CS pipeline. I want to know a safty and pratical method for lining and/or coating.
Feb 27, 2006 #2 dicksewerrat Civil/Environmental Joined May 16, 2002 Messages 1,946 Location US What kind of Q's and pressures? Richard A. Cornelius, P.E. http://WWW.amlinereast.com Upvote 0 Downvote
Feb 27, 2006 Thread starter #3 HXLIU Mechanical Joined Dec 5, 2005 Messages 6 Location CN Thanks a lot! The flowrate is 27000m3/h, the design pressure is 0.6 MPa. Upvote 0 Downvote
Feb 28, 2006 #4 civilperson Structural Joined Jan 13, 2006 Messages 2,399 Location US Coal tar epoxy lining will work in this application. The thicker the coating, the longer the survival of the pipe. Upvote 0 Downvote
Coal tar epoxy lining will work in this application. The thicker the coating, the longer the survival of the pipe.
Feb 28, 2006 #5 dicksewerrat Civil/Environmental Joined May 16, 2002 Messages 1,946 Location US Have you looked at GRP or HDPE? Richard A. Cornelius, P.E. http://WWW.amlinereast.com Upvote 0 Downvote
Mar 14, 2006 #6 Robfitter Specifier/Regulator Joined Feb 14, 2006 Messages 4 You should be okay with coal-tar epoxy, how long a run is it? The other thing might be to slipline it with HDPE. Upvote 0 Downvote
You should be okay with coal-tar epoxy, how long a run is it? The other thing might be to slipline it with HDPE.