Depending on what you are actually using the WPS for, this may just be a matter of semantics or you could recording the wrong thing. You shouldn't be using information from the WPS to fill out the WPQ, other than recording the identification of the WPS(s) used by the welder for qualification. The other values recorded on the WPQ have to be the actual values used by the welder qualificaiton during the test, not values from the WPS. However, you neeed to check these values to make sure they are in conformance with the WPS(s).