Jul 21, 2005 #1 DJKeng Mechanical Joined Jun 13, 2003 Messages 28 Location US I've been unable to find any tensile and yield strength listed for this alloy and temper of aluminum. can anyone point me in the right direction?????
I've been unable to find any tensile and yield strength listed for this alloy and temper of aluminum. can anyone point me in the right direction?????
Jul 21, 2005 1 #2 NickE Materials Joined Jan 14, 2003 Messages 1,570 Location US From the ASM metals handbook desk edition: For extruded wire, bar, rod, or shapes: 6105-T5 -- for dia up thru 12.70mm; Min UTS: 262MPa Yeild: 241 MPa ; min elong: 10%. Upvote 0 Downvote
From the ASM metals handbook desk edition: For extruded wire, bar, rod, or shapes: 6105-T5 -- for dia up thru 12.70mm; Min UTS: 262MPa Yeild: 241 MPa ; min elong: 10%.
Jul 21, 2005 Thread starter #3 DJKeng Mechanical Joined Jun 13, 2003 Messages 28 Location US thanks nick Upvote 0 Downvote
Jul 21, 2005 #4 Flesh Materials Joined Jul 17, 2003 Messages 108 Location US The minimum values NickE stated are also good up to 1 inch, per ASTM B221. Upvote 0 Downvote