I need a code or standard specify the maximum value of hardness after PWHT on P1 materials.
In many specs. it is 200 BHN but no official reference has been mentioned.
 
NACE MR0103, 2.1.7/ ISO 17945, 13.1.6.2 for stress relief of cold formed items

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
NACE SP 0472
API RP 582

These are recommended practices and standard practices. I believe they limit the hardness to 200 BHN in cracking environments, otherwise it is 225 BHN.
 