I need help finding a reference for the hardness values of Material 1.6368 (15NiCuMoNb5-6-4).


Appreciating your help
Thanks and Regards.
M Elsayed
 
Could you quote a US equivalent?

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 
200 to 210 Brinell.ASTM-A182-Grade-F36 is the similar alloy


luis
 