May 23, 2022 #1 TOMMY2010 Structural Joined Nov 1, 2020 Messages 18 Location OM Dear Gents, Hope you are all well! I need help finding a reference for the hardness values of Material 1.6368 (15NiCuMoNb5-6-4). Appreciating your help Thanks and Regards. M Elsayed
Dear Gents, Hope you are all well! I need help finding a reference for the hardness values of Material 1.6368 (15NiCuMoNb5-6-4). Appreciating your help Thanks and Regards. M Elsayed
May 24, 2022 #2 Guest Could you quote a US equivalent? "Everyone is entitled to their own opinions, but they are not entitled to their own facts." Upvote 0 Downvote
Could you quote a US equivalent? "Everyone is entitled to their own opinions, but they are not entitled to their own facts."
May 25, 2022 #3 0707 Petroleum Joined Jun 25, 2001 Messages 3,460 Location PT 200 to 210 Brinell.ASTM-A182-Grade-F36 is the similar alloy luis Upvote 0 Downvote