Mech_Guy_98
Mechanical
Hello Friends,
I need a clarification on below issue.
If we are providing 45mm thk end plate for an Header or pipe in fabrication drawing. But in Shop, available thickness is 50mm only.so they are machining the plate material to 45mm thick from 50mm thick plate.
Whether ASME code allows to machine the Plate materials?
Can anyone Suggest on this issue
Material used: SA 515 GR.60 /SA 516 GR.70
Regards,
R. Ilanseran
I need a clarification on below issue.
If we are providing 45mm thk end plate for an Header or pipe in fabrication drawing. But in Shop, available thickness is 50mm only.so they are machining the plate material to 45mm thick from 50mm thick plate.
Whether ASME code allows to machine the Plate materials?
Can anyone Suggest on this issue
Material used: SA 515 GR.60 /SA 516 GR.70
Regards,
R. Ilanseran