This is a strange occurance for me. Does anyone have any experience with this? The engine has been assembled as many before it have. here are the details
2000cc
I4
tubocharged GT3076R (the real one)
15psi boost.
engine has run for 350 miles
cyls 1-3-4 have ~140psi evenly
cyl 2 is running 84psi when cold and has only 30psi when warm
this was veryified by 2 technicians and 4 different guages.
there is a deffinite leak past the rings when leak tested on cyl 2.
the cylinder walls were coated with anti friction coating and i am hoping this is just causing the rings not to seat properly.
strangely engine does not appear to have a balace problem while running.
any advice with 84 cold and 30 hot would be nice. i am going to try a few more psi boost to see what happens.
after that it will come apart for inspection anyway.
2000cc
I4
tubocharged GT3076R (the real one)
15psi boost.
engine has run for 350 miles
cyls 1-3-4 have ~140psi evenly
cyl 2 is running 84psi when cold and has only 30psi when warm
this was veryified by 2 technicians and 4 different guages.
there is a deffinite leak past the rings when leak tested on cyl 2.
the cylinder walls were coated with anti friction coating and i am hoping this is just causing the rings not to seat properly.
strangely engine does not appear to have a balace problem while running.
any advice with 84 cold and 30 hot would be nice. i am going to try a few more psi boost to see what happens.