Our plant using a ceramic fiber blanket used to insulated steam line. During instalation the insulation was exposed to heavy rain water. The fiber insulation is severely wet because of that.
My question:
-should we replaced the insulation? what is the cause? Can we just put it in dryer to remove the water?
- some people say the insulation contain chloride that can enhance corrosion in piping system. It is true?
- could someone give me any insulation practice literatur?
Thanks for all of your help
devaxrayz
process engineer
Our plant using a ceramic fiber blanket used to insulated steam line. During instalation the insulation was exposed to heavy rain water. The fiber insulation is severely wet because of that.
My question:
-should we replaced the insulation? what is the cause? Can we just put it in dryer to remove the water?
- some people say the insulation contain chloride that can enhance corrosion in piping system. It is true?
- could someone give me any insulation practice literatur?
Thanks for all of your help
devaxrayz
process engineer