I have Sec II Part D 2004 and do not find Inconel 718 (N07718) nor x750 (N07750) both of which would be SB637. I am interested in bar stock.

Is this in the later editions? What I need is allowable stress at 100F and also the max temp.

Any help will really be appreciated.

Paul

 
YBM, neither is listed 2011 Addenda

Regards,

Mike
 
Inconel 718 and X750 are listed under bolting materials in Table 3 of Part D. See SB-637.
 