Hello Friends

Material: SA 387 GR 21, CL 1 Thickness: .350", MDMT 10°F 200 psig
is that i need IMPACT TESTING.

 
Very much depends on Code of Construction, if any.

Regards,

Mike

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
ASME section viii div 1
 
my understanding yes.
UCS 66 - FIG- M.D.M.T VS THICK - Point locate above curve B
any opinion please.
Regards
stan
 
Based on the limited information you've provided please look at Table UCS 66 Curve B materials up to 11/16" thick are exempt to +10 F
 
as per table UCS-66M, for SA 387 grade21 curve C is applicable.

the combination of MDMT & THICKNESS comes above curve C. Hence impact is not applicable.
 
Just a clarification:

SA-387 Gr 21 and Gr 22 belong to curve C, IF normalized and tempered or liquid quenched and tempered. See Figure UCS-66 note (3)(a).

Regards.
 
yes it will be ON curve A BECAUSE IT IS PLATE.
NOT ON CURVE C. I Thought first will be on curve B.
NOW REGARDING SA 387- P3 group
ucs 66 MDMT & thickness curve - INTERSECTION POINT is below curve A. SO YES NEED IMPACT TESTING.

REGARDS
stan
 
So your plates must be annealed? If they are not, they must be normalized and tempered or liquid quenched and tempered per SA-387....and would then be Curve C as Jano6924 pointed out.
 
stan000 (Mechanical)
(OP)
SA 387 is plate specification. It belongs to curve C only.


the combination of MDMT & THICKNESS comes above curve C. Hence impact is not applicable.


You may like to recheck your statement.
 