Impact Test Requirement as per ASME SEC8 DIV3

Status
Not open for further replies.

Ronak_Patel

Mechanical
Joined
Jul 26, 2021
Messages
44
Location
IN
Hello All,

As per KM-251 in DIV3 : "The Charpy V-notch impact values specified in KM-234.2 are established at upper shelf energy levels that are required for most high-strength, low-alloy steels. The designer does not need to provide any test information to use upper shelf correlations for these materials."

KM-234.2 Specify 68 J for avg of 3 specimens in Long Direction.

I'm bit confused with KM-251 statement. from KM-234.2 requirement, I understand that material shall as min have 68J energy value at MDMT temp.

Is this 68J shall be Upper shelf energy value for material as per KM-251??
 