Hi all,
I have a vessel, having an MDMT of -44 Deg C. I am using SA 516 70 for shell and heads. The design pressure is 98 bars at which the thickness of shell and heads is coming as 106mm. Since, the impact test is mandatory, should I ask the vendor to take normalized material or is there no requirement of normalizing the material since it is to be impact tested?
I have a vessel, having an MDMT of -44 Deg C. I am using SA 516 70 for shell and heads. The design pressure is 98 bars at which the thickness of shell and heads is coming as 106mm. Since, the impact test is mandatory, should I ask the vendor to take normalized material or is there no requirement of normalizing the material since it is to be impact tested?