I am looking for the tensile and yield values for AISI 1045 (ASTM A576 1045) carbon steel at 200 degrees C. Can anyone help?
 
Other than actual published elevated temperature test data for 1045 carbon steel (supplied with no heat treatment), I would suggest an approach where knock down factors for each test temperature have been established based on elevated temperature mechanical property data for structural steels. The key is that most carbon steels will follow a similar trend curve for elevated temperature mechanical properties.

You can search the Internet for publications related to
"mechanical properties of several structural steels at elevated temperatures"
 