Does anyone have any experience with hydroexpanding (instead of a plain roll) heat exchanger tube to tubesheet joints? We currently roller expand our joints and still have leakage problems which forces us to then add a strength weld. I am hoping that hydroexpanding will eliminate a strength weld.
Any input would be great!
Thanks
Any input would be great!
Thanks