Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

How to Qualify Inconel 625 CRO onto 316L SAW on 516 Gr 70

Status
Not open for further replies.

normankiddie

Mechanical
Joined
Jan 28, 2007
Messages
5
Location
US
I have a Question on how Qualify Inconel 625 CRO (Automated GMAW) onto 316L Strip Welded SAW on 516 Gr 70 Plate. I have a client that needs to have his 3mm 316L cladding overlayed with 3mm of Inconel 625, I use automated GMAW. The question has now surfaced, how does one qualify it:
1) On SA 516 Gr 70,
2) On SA-240 Gr 316L or
3) Does one Overlay 516 with 316L and do it that way.....
The cladding will be on 20" and smaller Nozzles, so delamination is not a concern.........
 