I have a plastic tube design with either a hexagonal or octagonal
cross section. Wall thickness is constant. Overall, part is 3" long, 0.48"
major diameter, 0.02" wall. The twist is that the cross section forms a
helical path with a desired constant pitch of between 0.5 to 3.0. The
most important aspect to keep is the internal helix .
I can get a decent prototype with SLA or ABS plastic (fused deposiiton?). I wanted a
smooth metal working model, but machine shops tell me it is not within
their capabilities [ including swiss screw machines]. Assuming any
plastic, anybody know how this can be mass produced ? I have
an Injection Molding quote, but tooling costs are steep. I'm leaning
towards extrusions. But, so far Extruders have nixed it ["haven't done
an internal helix"] Any ideas?
*
*
*
cross section. Wall thickness is constant. Overall, part is 3" long, 0.48"
major diameter, 0.02" wall. The twist is that the cross section forms a
helical path with a desired constant pitch of between 0.5 to 3.0. The
most important aspect to keep is the internal helix .
I can get a decent prototype with SLA or ABS plastic (fused deposiiton?). I wanted a
smooth metal working model, but machine shops tell me it is not within
their capabilities [ including swiss screw machines]. Assuming any
plastic, anybody know how this can be mass produced ? I have
an Injection Molding quote, but tooling costs are steep. I'm leaning
towards extrusions. But, so far Extruders have nixed it ["haven't done
an internal helix"] Any ideas?
*
*
*