Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

How is this assembled?

Status
Not open for further replies.

Abhinav89

New member
Joined
Aug 10, 2015
Messages
2
Location
IN
Hello Everyone!

I have been trying to develop a product which requires the assembly of a silicone slit valve in a plastic component.
I purchased a products containing this assembly but I can't seem to figure out how it is done.
The picture below show what I am trying to achieve.

IMAG0118_ddaivp.jpg


The plastic is one single piece. I was assuming the silicone would be pinched between two snap fitted plastic pieces but it is not the case.
I am assuming that the same principle would apply to the following assembly:
(Please correct me if I'm wrong [smile])

IMAG0119_cdgq21.jpg


Any advice will be helpful.

Thanks!
Abhinav
 
It could be a two-shot moulding where the elastomer material is moulded onto the part. Usually requires an elastomer which bonds to the base material. It might not be silicone in this case, more likely to be a TPE.

www.tynevalleyplastics.co.uk

Politicians like to panic, they need activity. It is their substitute for achievement.
 