How could I find equivalent European materials vs ASTM?

Status
Not open for further replies.

wangzh2k

Mechanical
Dec 12, 2007
28
Hi all,

Is there anyone knowing the European materials vs ASTM material such as A182-316L corresponding European SS material?

Thanks in advance.
 
Replies continue below

Recommended for you

European standard EN 10222-5 is for stainless forging materials. This standard includes material No. 1.4404 which is similar stainless steel with low-carbon content as 316L. See websites of European material manufacturer's.
 