Hello,
I have noticed that many companies do not utilize high yield pipe (e.g. API 5L Grade X42) in their pipe specs for facilities that will conform to B31.3. However, the same companies do utilize high yield pipe in their specs for facilities conforming to B31.8.
Is there a reason that high yield pipe is avoided for B31.3 facilities?
It seems that it would allow using STD instead of XH in certain sizes/pressure classes, which would save a bit of money.
I have noticed that many companies do not utilize high yield pipe (e.g. API 5L Grade X42) in their pipe specs for facilities that will conform to B31.3. However, the same companies do utilize high yield pipe in their specs for facilities conforming to B31.8.
Is there a reason that high yield pipe is avoided for B31.3 facilities?
It seems that it would allow using STD instead of XH in certain sizes/pressure classes, which would save a bit of money.