Dear all,

A very good day to you. I have a confusion regarding heat treatment of welded WPB wrought fittings manufactured to BPV section II Part A: 2017.
When welded wrought fittings of Grade WPB of nominal thickness > 19mm, are manufactured by welding of cold rolled two half plates/shells; is it necessary to:
a. Normalize or stress relieve the whole fitting including body and weld as per clause 7.2.4 of SA 234?
b. Stress relieve only the weld as per section 7.2.5 of SA-234?

 
Replies continue below

Recommended for you

Are you an end user, or manufacturer?

If you are an end user, what has been done the fitting in question?

The devil is in the details; she also wears prada.
 