Hi everyone. We are starting a develop of valves with iconel head, the problem here is get the best parameters for grinding this kind of material, Does anyone have any idea of the problem we will have doing our job??
We have had a very good experience in using high-porous vitrified CBN wheels for grinding Inconel. These wheels do not clog and grind a way cooler. Contact me for more detailes. gurinovich@abrazive.spb.ru