Grain size method for Al-castings

Status
Not open for further replies.

Flesh

Materials
Jul 17, 2003
108
Which method from ASTM E112 is typically used (by the foundry's lab) to measure grain size in aluminum castings? Is ASTM E112 the correct standard to use in this case (Al-castings)?
 
Replies continue below

Recommended for you

The linear intercept method is probably the most frequently used method from ASTM E 112. Image analysis techniques are starting to replace the manual methods.
 