Hi,

I have a drawing that calls out ASTM E1417 Type I method A, form d, class 2. Is solvent remover class only specified on ASTM E1417 Type I, Method C or could it be specified if "form d" (nonaqueous) developer is used?
 
kevlar49,

Solvent removable is Method C. (You are only going to do solvent removable with Type II inspections (visible)). Method A is water washable. There is no solvent remover used with water washable penetrants.

Jr97
 