AT one time I had a series of publications from Carpenter, one of which dealt with the Galling of Stainless Steels. It described the performance of different combinations in contact.

I have no idea what happened to them.

Does anyone know if this publication is available anywhere, or even similiar publications?

Thanks!

Paul
 
Replies continue below

Recommended for you

Have you tried going to Carpenter's web site and looking for it?
 
Yes, I could not find it online.

Being it is the weekend, I cannot call until tomorrow. It is a shame in that many companies have stopped publishing on paper, but they did not put these valuable resources on line either.

But then, I am the one who lost his copies.....

Paul
 
monkeydog and RPstress

These are helpful. I quick read shows me that this is similar to what was in the pub. that I referenced.

I will also continue to try to collect (recollect) some of that information.

Thanks to both of you.