Filler recommendation for welding P9 to Inconel 600

Status
Not open for further replies.

timsch

Mechanical
Oct 27, 2009
194
From searching posts on this forum, I gather that there is no particular source for filler metal selection for dissimilar metals, and is left to designer discretion. I understand that the selection of filler is usually based on the higher strength material and chemistry should closely match that.

In my case, I'll match the Inconel, which from my experience would usually be a Inconel-82 or -625 filler. How would you understand when to choose one over the other for any given situation? I don't have process info, but could get it.
 
Replies continue below

Recommended for you

Nickel base filler metals would be used for all nickle base alloys to ferritic materials. The selection should be based on service conditions.
 