Existing Steel Stair Assesment: Rivet and Bolt size vs. head dimension?

Status
Not open for further replies.

KirkGH

Structural
Joined
Jul 17, 2008
Messages
29
Location
US
I'm assessing an existing 4 story fireescape stair. I can't get an exact year of construction, but based on the evidence presented we're going to assume 1927.
I measured the heads and diameter where I could and here's what I'm left with.

Bolts (square head):
.394"dia. .... head
... dia. .84" head
... dia. .605" head
1" dia. .... head
1/2" dia. .... head

Rivet:
... dia. .70" head
.50" head
.88" head

I need some help converting these approximate 1927 head sizes to diameters. Any guidance?

I got material strengths from AISC design guide 15 for a conservative 25 ksi yield and 46 ksi ultimate on the steel.

For rivets I can get an ALLOWABLE 1928 value of 13.5 ksi tension and shear. But this tells me nothing about the nominal stress I need for current AISC. Any guidance?

For bolts I can get an ALLOWABLE 1936 value of 10 ksi shear. But this tells me nothing about the nominal stress I need for current AISC. Any guidance? I'm tempted to just use the old allowable values with the new allowable load criteria of current Code.

Thanks.
 
Why don't you just check vs. allowable? Don't try to fit a square peg in a round hole.
 