As far as I know all Eucalyptus grown in South America have come originally from Australia. There are many species and the properties are in the Australian Standard AS 1720.2 ...available over the internet from Standards Australia. (metric standard)
You must know the species and the grading to assign most properties. Of course, as you know, the growing conditions are different to the native forests in Australia and so the properties may be better or worse. You would need to test in-grade to verify properties.
I would be surprised if testing of this timber has been already carried out in your country.