Oct 10, 2023 #1 SMKRe Mechanical Joined May 17, 2023 Messages 44 Location IN What is the emissivity of 17CrNiMo6/18CrNiMo7 material for the temperature range of 0 deg C to 150 deg C?
What is the emissivity of 17CrNiMo6/18CrNiMo7 material for the temperature range of 0 deg C to 150 deg C?
Oct 11, 2023 #2 0707 Petroleum Joined Jun 25, 2001 Messages 3,444 Location PT Dificult question try to google. Upvote 0 Downvote
Oct 12, 2023 #3 btrueblood Mechanical Joined May 26, 2004 Messages 10,033 Location US Because it varies extensively depending on the degree/depth of oxidation the surface has. Heavily weathered/oxidized it will be up around 0.8 or 0.9. Polished under argon and tested in vacuum, it will be low, maybe 0.1 to 0.2. Upvote 0 Downvote
Because it varies extensively depending on the degree/depth of oxidation the surface has. Heavily weathered/oxidized it will be up around 0.8 or 0.9. Polished under argon and tested in vacuum, it will be low, maybe 0.1 to 0.2.
Oct 12, 2023 #4 M MintJulep Mechanical Joined Jun 12, 2003 Messages 10,242 Location JP And it's not likely to be constant over this temperature range. Upvote 0 Downvote