Thanks, Unk...
I've specified a two part polyurethane coating from Euclid Chemicals in past... with good results, and I had a query from a contractor about specifying a second product and was wondering if anyone else had a good product they had used. It's for a concrete slab and my experience is that polyurethanes hold up much better than acryllic coatings...
Dik