Hello all. I'm very interested in working with carbon fiber for automotive applications. My goal is to produce aesthetic and structural pieces. I think I've decided on vacuum infusion since I can't afford a large autoclave for pregreg. But before I go out and buy equipment and materials, I want to practice making molds first. I would very much like to use plaster molds versus fiberglass, but I'm not sure whether or not it is a suitable material for vacuum-infusion carbon fiber. If it is, what type would you recommend?

Any information you have would be greatly appreciated!
 
Have you tried to obtain information from resin, prepreg and fibre suppliers.

Have you tried doing a google search.

Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
I've been looking for information. It seems like fiberglass is popular for molds. I don't see why plaster wouldn't work, but I've never worked with composites, let alone carbon, so I thought I would seek out people that have more experience
 
Whether fibre glass and carbon fibre, it makes no difference to the mould.

Fibre glass moulds will be a lot lighter and stronger than plaster.

It will be difficult to get good mould release from a plaster mould, so a lot of mould release wax might be needed. This might reduce the surface gloss and therefore require more effort in the finishing of the part.

Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
You will have reliability/structural issues using plaster as a mold. It is handy for taking a 'splash', but I always build my molds out of something more robust.
 