Codes governing use of fiber reinforced plastic structural shapes 2

Status
Not open for further replies.

stanweld

Materials
Joined
May 9, 2003
Messages
2,906
Location
US
Are there any codes governing construction of buildings or other structures using fiber reinforced structural shapes?

 
stanweld;
ASME Boiler and Pressure Vessel Code Section X - Design and Construction of Fiber Reinforced Plastic Pressure Vessels

For Repair -refer to the 2004 Edition of the NBIC
 
metengr,
Thanks for the quick response; unfortunately, that is the Code with which I am familiar. The codes that I am interested in would govern construction of buildings, bridges, cooling towers, tank supports, etc.

 
Check out the manuals from Strongwell Corporation. They have several design manuals with load tables and other information based on their product line.


In structures there is not a great deal of information as of yet to really have a standard design code. The ACI has several publications concerning the use of FRP bars for reinforced concrete also, but I don't think they have made it to being called "codes" yet either.
 