metengr,
Thanks for the quick response; unfortunately, that is the Code with which I am familiar. The codes that I am interested in would govern construction of buildings, bridges, cooling towers, tank supports, etc.
Here is one supplier that we used for structurals around a plant that used HCl. They were very good with information at one time. The also have a lot of info available on their web site.
Check out the manuals from Strongwell Corporation. They have several design manuals with load tables and other information based on their product line.
In structures there is not a great deal of information as of yet to really have a standard design code. The ACI has several publications concerning the use of FRP bars for reinforced concrete also, but I don't think they have made it to being called "codes" yet either.