MikeG7, carbon steel SA-516-70, SA-350-LF2, etc. could be used in the application, but the allowables will take a hit. Hydrogen service should not present any special problems from a material standpoint, but fabrication details are important, especially avoidance of unvented crevices. Stainless clad should be OK.
Cladding should not be included in the thickness for Part UHX calculations. It can be treated as corrosion allowance although this presents some difficulties such as when a pass groove is used, and with any uncorroded output data.
Can't remenber offhand but your design temp may put you in the time-dependent property region, if so, particular requirements in allowables and in Part UHX calculations come into play.
Maybe a lo-alloy would be a better choice.
Regards,
Mike