Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Choose Holding Temp. for P5A + P15E using welding material Type 22 i.e 21/4Cr 1Mo

Status
Not open for further replies.

WinWin2022

Mechanical
Joined
Nov 17, 2022
Messages
3
Location
VN
Hey Sir/Madam,
When manufacturing at shop, we detected that have one case as bellow:
Item Header in Boiler has some noted:
- Bent stub SA213 T91. Post bend heat treatment Temp. range: 745~775 degree C
- Pipe SA335 P22 + Stub SA213 T91. As WPS Post weld heat treatment temp. range: 720~740
- Pipe SA335 P22 + Pipe SA335 P22. As WPS Pwht temp. range: 680~740
- Pipe SA335 P22 + Ins. Nozzle SA182-F22-3. As WPS Line Pwht temp. range: 720~740

=> For this item to be Whole PWHT, we will revise 3 WPS above and Bending Procedure with temp. range is 730 ~ 750.
We don't know base metal P5A + P15E using welding material Type 22 i.e 21/4Cr 1Mo holding temp. 730~750 is right or wrong?
If holding temp. in range 730~750 is matching with ASME Code Sec.I PG-20 & Table PW-39.2, but using welding material Type 22 i.e 21/4Cr 1Mo have make reduce welded strengh of welded?
Thank you and happiness when receive your feedback.
 
There will be no loss of strength with respect to the base metal minimum requirements when the filler metal is 2 1/4 Cr - 1 Mo alloy as defined in the various SFA specs.
 
Status