Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JAE on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Carolina Roller Coaster shutdown due to large crack spotted by park guest.

Status
Not open for further replies.

Cool_Controls

Electrical
Joined
Feb 5, 2020
Messages
166
Location
US
Link
Thankfully not a disaster, but their inspection process will certainly be questioned. Is routine NDT something that is performed on amusement rides?
b9c8a012-19e8-47e0-8733-5592c8725f90_1140x641_hjb6cg.jpg
 
Wow ! The owner of that ride should be paying the person that reported that, and the insurance company as well.
I'd like to know if that is some nice computer aided design of that area?
The post behind it is the same design. That design failed its test, it is due for a complete redesign.
Shows why the support should be at that top area and in compression, meaning the opposite side for that diagonal brace.
It looks like the brace upper weld is the point of the stress riser.
I don't plan to ever ride on any thing like that, though I have in the past.
 