I am interested in finding a BPA free alternative for a juvenille beverage container. The product will be injection molded, come in varied translucent colors and need to have a decent impact resistance. Suggestions?

Thanks in advance
 
Replies continue below

Recommended for you

I would avoid SAN due to poor impact resistance. Impact modified, transparent SAN (like MABS) would work as would the other suggestions. If you don't need perfect transparency then the PP route will be nice from a materials cost standpoint.

Chris DeArmitt

"Knowledge has no value except that which can be gained from its application toward some worthwhile end."