Jun 22, 2011 #1 LiBrown Chemical Joined Jun 22, 2011 Messages 2 Location DE What is an effective adhesive for bonding Polyetheretherketone (PEEK) film? I am using plasma as a pre-surface treatment. The application is high pressure and with water.
What is an effective adhesive for bonding Polyetheretherketone (PEEK) film? I am using plasma as a pre-surface treatment. The application is high pressure and with water.
Jun 22, 2011 #2 btrueblood Mechanical Joined May 26, 2004 Messages 10,034 Location US Epoxy. Upvote 0 Downvote
Jun 22, 2011 #3 Compositepro Chemical Joined Oct 22, 2003 Messages 7,846 Location US I agree with epoxy. Upvote 0 Downvote
Jun 23, 2011 1 #4 patprimmer New member Joined Nov 1, 2002 Messages 13,816 Location US Victrex literature says epoxy. It says cleaned with solvent then dried. It says surface roughening, flame treatment or etching with chromic acid all improve the bond strength, flame by about 20% and chromic by about 30%. Epoxy resins give from 0.45 to 5.38mpa bond strength depending on type, surface preparation and method of application. Hylobond F300 AB 450 CA30 on a solvent cleaned and 80 grit sandblasted surface gave best results. Regards Pat See FAQ731-376 for tips on use of eng-tips by professional engineers & http://eng-tips.com/market.cfmfor site rules Upvote 0 Downvote
Victrex literature says epoxy. It says cleaned with solvent then dried. It says surface roughening, flame treatment or etching with chromic acid all improve the bond strength, flame by about 20% and chromic by about 30%. Epoxy resins give from 0.45 to 5.38mpa bond strength depending on type, surface preparation and method of application. Hylobond F300 AB 450 CA30 on a solvent cleaned and 80 grit sandblasted surface gave best results. Regards Pat See FAQ731-376 for tips on use of eng-tips by professional engineers & http://eng-tips.com/market.cfmfor site rules