In our application, we are using something that looks like a baloon with two inputs, the volume is ~100 mL
currently this item is made using a silicon dispersion and a ptfe Master is put in this bath 15 times with pauses to get the correct 0.2mm thickness The whole process takes less than a minute of handwork but roughly a day of curing.
Now that the product is having some success our concern is that we will need 10k lots ...
Any tips & ideas of a better manufacturing process ?
Thanks,
HS
currently this item is made using a silicon dispersion and a ptfe Master is put in this bath 15 times with pauses to get the correct 0.2mm thickness The whole process takes less than a minute of handwork but roughly a day of curing.
Now that the product is having some success our concern is that we will need 10k lots ...
Any tips & ideas of a better manufacturing process ?
Thanks,
HS