Apr 17, 2007 #1 redandysafc Mechanical Joined Dec 18, 2005 Messages 60 Location GB If my welders are coded to weld stainless steel with wire on a butt to ASME IX are they coded to weld a butt with no wire.
If my welders are coded to weld stainless steel with wire on a butt to ASME IX are they coded to weld a butt with no wire.
Apr 17, 2007 1 #2 weldtek Materials Joined Feb 12, 2005 Messages 897 Location US GTAW, No. See QW 404.14 Upvote 0 Downvote
Apr 17, 2007 Thread starter #3 redandysafc Mechanical Joined Dec 18, 2005 Messages 60 Location GB So that means No Cheers Upvote 0 Downvote